Performed mainly for the aeronautical industry, it is applied on titanium or stainless steel as well as on primary light alloy parts.
Substrate
Performed mainly for the aeronautical industry, it is applied on titanium (treated or not) or stainless steel as well as on primary light alloy parts that have undergone one of the following treatments:
Chromic anodizing (BF5), not sealed
Chromic anodizing (BF5), sealed
Alodine 1200
Pickling
Paints used
PU 66 d(PPG)
AERODUR SGL (AKZO)
S15/90 (AKZO)
Hydrodiluable (MAPAERO, etc.)
Bonding primers
On unsealed chromic anodic oxidation
On pickled parts
At the customer’s request according to the same procedure as paint
The most commonly used are: Redux 112, 113, 119 and 122, BR 127 and 227 (Airbus), and METLBOND 6726 (helicopters)
Results
Paint thicknesses are precise. The work of painters is organized with self-inspection; the finished parts being of course subject to the approval of the inspection department.