2.3 – 4.2 µm, three-stage thermoelectrically cooled
PV-3TE-4 is three-stage thermoelectrically cooled IR photovoltaic detector based on sophisticated HgCdTe heterostructure for the best performance and stability. The device is optimized for the maximum performance at λopt = 4.0 μm. Cut‑on wavelength can be optimized upon request. Reverse bias Vb may significantly increase response speed and dynamic range. It also results in improved performance at high frequencies, but 1/f noise that appears in biased devices may reduce performance at low frequencies. 3° wedged sapphire (wAl2O3) window prevents unwanted interference effects.
Features:
- High performance in the 2.3 - 4.2 µm spectral range
- Three-stage thermoelectrically cooled
- No bias required
- No 1/f noise
Parameter: PV-3TE-4
Material: MCT
Type: Photovoltaic
Immersion: Non-immersion
Cooling: Three-stage
Wavelength/ λopt/ µm: 4
Package: TO8, TO66
Window: wedged Al2O3
Detectivity/D∗/cm⋅Hz1/2⋅W−1: ≥4,0x1010
Time constant/ τ/ ns: ≤100