●Material:6J13 manganin and copper with high resistivity and low temperature;
●Welding types: Electro-beam welding and overlap welding;
●LowTCR(temperature coefficient of resistance )value with temperature variation;
●All the shunt will be processed with temperature Aging: 10 hours under 120 deg;
●Customised design according to clients requirement, 200,250,300,350,400,500μΩetc, they can be amounted on terminal block ·with screw holes fixed, also can bewelded with others copper links or copper braid
●Tolerance standard+5%;
●Both the wires and pins connection to PCB can be customised designed;
●Good linearity;
●Cost Effective;